Abstract

Low loss Mg2TiO4 (MTO) ceramics have been synthesized by mechanical synthesis method. The effect of processing parameters, on initial particle size, microstructure, relative density, and microwave dielectric properties of MTO ceramics are investigated. The maximum relative density was obtained 97.75%, and uniform microstructure is observed for the sample sintered at 1325°C for 3 h. The driving force for the sintering can be attributed to the surface energy of fine powders and their defect energy. There is not much variation in dielectric constant (εr) where as Q × fo is affected and the values of Q × fo are in the range of 99,500–155,500.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.