Abstract

PbZr 0.53Ti 0.47O 3 (PZT) thin films with thickness of 0.9 μm were prepared on La 0.5Sr 0.5CoO 3 (LSCO) coated Si substrates. Both PZT and LSCO were prepared by the sol–gel method. The concentration of LSCO sol was varied from 0.3 to 0.1 mol/L, which could modify the preferential orientation of PZT thin films and consequently affect the dielectric and ferroelectric properties. The LSCO electrode layers derived from lower sol concentration of 0.1 mol/L have much more densified structure, which facilitates the formation of (1 0 0) textured PZT films with smooth and compact columnar grains. PZT thin films prepared on the optimized LSCO films exhibit the enhanced dielectric constant and remnant polarization of 980 and 20 μC/cm 2, respectively.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.