Ultra-thin gate oxide reliability, in large area MOSFETs, can be monitored by measuring the gate current when the substrate is depleted. When the channel length is scaled down, the tunneling current associated with the source/drain extension region (SDE) to the gate–overlap regions can dominate the gate current. In N-MOSFETs, as a function of the negative gate voltage two components of the gate–drain leakage current should be considered, the first for V FB < V G < 0 V and the second for V G < V FB. These components are studied in this work before and after voltage stresses. The aim of this work is to see whether this gate–drain current can be used to monitor the oxide degradation above or near the source and/or drain extension region in N-MOSFETs. It is important because the most serious circuit-killing breakdown occurs above or near the drain (or source) extension region. Finally, we show that it is necessary, before explaining the gate LVSILC curves obtained after stresses on short-channel devices, to verify which is the dominate current at low voltage.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.