This paper presents the results of an examination of cracking discovered in stainless steel anchors in a refractory block destined for inclusion in an ignition hood. Cracking was found to be a result of stress corrosion cracking due to exposure to chlorides from the breakdown of PVC electrical tape in which the anchors had been wrapped to form an expansion coating during the curing of the refractory material into which the anchors were inserted.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.