Abstract Stress corrosion cracking (SCC) behavior in 60% Ca(NO3)2, 3% NH4NO3 solution boiling at 110 C is reported for relatively pure 1% Ni, 1% Cr, or 1% Ti steels as a function of carbon content. The steels were water-quenched, cold-rolled, or furnace-cooled. Commercial 4140 steel heat-treated to various hardness levels was similarly tested. It was also subjected to SCC in boiling 3% NaNO3 and boiling 3% NaCl. Critical potentials below which SCC does not occur were measured in 3% NaNO3 for the latter steel at 4 hardness levels. The results are interpreted in terms of stress-sorption cracking.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.