Abstract

Abstract The stress corrosion cracking (SCC) susceptibility of Zr (UNS R60702), Zircaloy-4 (UNS R60804), and Ti (UNS R50400) in a 10-g/L iodine-methanol solution was studied. SCC, always preceded b...