Stress corrosion cracking of austenitic stainless steels by sulfur compounds has been investigated and the following results are obtaind;(1) Austenitic stainless steels were subjected to stress corrosion cracking in solution of sulfurous acid and solution of sulfurous acid and polythionic acids when the Cr impoverished zone existed around the grain boundaries.(2) Sulfite solution or polythionates solution did not induce the stress corrosion cracking failure.(3) The stress corrosion cracking were observed to be intercrystalline by optical and electron microscopy.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.