Abstract
In this study, the stress corrosion cracking behavior and bioactivity of Ti–Zr–Cu–Pd–Sn bulk metallic glass (BMG) were investigated. The results revealed that the Ti-based BMG exhibited similar tensile behavior in Hanks’ solution with a slightly lower strength than that in air. A bioactive surface layer composed of calcium phosphate compound was obtained after a two-step treatment on the Ti-based BMGs. Hydrothermal–electrochemical treatment was effective to form a porous surface layer by increasing the Ti content and decreasing the Cu content in the surface. Consequently, pre-calcium treatment accelerated the nucleation of calcium phosphate particles. After hydrothermal–electrochemical and pre-calcium treatments, following by soaking in Hanks’ solution, homogeneous calcium phosphate layer formed on the Ti-based metallic glass.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.