Abstract

The fracture kinetics of Al-5.5 Zn-2.5 Mg alloys submersed in 3 pct NaCl-H2O solutions were varied by heat treatment. The steady state velocity, on a plot of velocity vs stress intensity, was compared with microstructure and it was found to be inversely proportional to the volume of MgZn2 in the grain boundary. This behavior suggests that grain boundary precipitates can act as sacrificial anodes to retard intergranular stress corrosion cracking.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.