Abstract

In order to study the relationship between thickness and residual stress in CaO−Al2O3−SiO2 glass-ceramics. The residual stress was measured in CaO−Al2O3−SiO2 system glass-ceramic with different thickness, and the formation mechanism and characterization of residual stress in CAS system Glass-ceramic were analyzed by the X-ray diffraction analysis. The experimental results show the compressive residual stress increases with thickness of glass-ceramic increasing.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.