Abstract

This paper presents the results of experimental research on full-size laminated veneer lumber (LVL) beams unreinforced and reinforced with CFRP sheets. The nominal dimensions of the tested beams were 45 mm × 200 mm × 3400 mm. The beams were reinforced using the so-called U-type reinforcement in three configurations, differing from each other in the thickness of the reinforcement and the side surface coverage. An epoxy resin adhesive was used to bond all the components together. A four-point static bending test was performed according to the guidelines in the relevant European standards. The effectiveness of the reinforcement increased with the level of coverage of the side surface and the level of reinforcement. The average increases of bending resistance were 42%, 51% and 58% for configurations B, C and D, respectively. The average value of bending stiffness increased for the beams of series B, C and D by 15%, 31% and 43%, respectively. Their failure mode changed from brittle fracture initiated in the tensile zone for unreinforced beams to more ductile fracture, initiated in the compression zone. The influence of the coverage of the side surface by the CFRP sheet and reinforcement ratio on the mechanism of failure and effectiveness of strengthening was studied in the article.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.