Abstract
Stud joints of 2017 aluminium alloy were friction welded and its joint strength was examined. A stair zone was formed at the weld interface. Although the hardness of the stair zone was almost the same as base metals, the heat-affected zone of the bar and the plate was softened. The tensile strength of joints tended to increase with a pressure and a friction time, and the highest tensile strength was 275 MPa (63.1% joint efficiency for the bar base metal). In the bending testing, joints were cracked in the weld zone at a bending angle of less than 5°. In the fatigue testing, joints fractured near the weld interface and the fatigue strength of joints increased as the tensile strength of joints was high.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.