Abstract
Copyright 1998 ASM International. This paper was published in Metallurgical and Materials Transactions A: PhysicalMetallurgy and Materials Science, Vol. 29.5, 1527-1530 and is made available as an electronic reprint with the permissionof ASM International. One print or electronic copy may be made for personal use only. Systematic or multiplereproduction, distribution to multiple locations via electronic or other means, duplications of any material in this paperfor a fee or for commercial purposes, or modification of the content of this paper are prohibited.Available on publisher's site at:http://www.asminternational.org/portal/site/www/AsmStore/ProductDetails/?vgnextoid=743cc777b3426210VgnVCM100000621e010aRCRD.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.