We have studied the domain structure formation in annealed BaTiO 3 films grown on SrTiO 3. We show that it is possible to utilize the 2.28% lattice mismatch strain at the SrTiO 3/BaTiO 3 interface to obtain uniaxially c-axis-oriented BaTiO 3 films with a thickness of up to about 200 nm. This thickness is much larger than the typical critical thickness for BaTiO 3 films on SrTiO 3 and such films therefore can potentially be useful for optical waveguide applications. We also looked at the polarization properties of the uniaxial BaTiO 3 films. Our measurements and analysis indicate that the heavily distorted interface region, with a thickness of approximately 2 nm is non-ferroelectric.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.