Abstract
The positive effects of deep rolling on fatigue strength-reduced surface roughness, work hardening and compressive residual stress-in the near-surface region are achieved by controlled high plasticisation of the treated material. However, excessive and/or repeated plasticising poses a risk of damage to the machined component. This paper investigates the damage caused by deep rolling of a railway axle. Two sections of the axle are experimentally deep rolled repeatedly at different feed rates until damage is detected. For comparative analysis, these experiments are numerically analysed and the damage is assessed using the strain-based damage calculation. The results are compared and a damage sum of ~120% is evaluated for both tests, thus developing a reliable and conservative assessment method. The single deep rolling treatment at a feed rate of 0.25 mm causes damage of 6.1%, and at a feed rate of 0.5 mm, damage of 4.7%. The developed and experimentally validated evaluation method allows for investigating the limits of applicability of different deep rolling parameters. The influence of the deep rolling force and feed rate and a proposed optimisation with multiple deep rolling with reduced deep rolling forces are investigated.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.