Abstract

Kenaf is an economically viable and ecologically friendly cellulose source. It can be used in the textile, paper, and bio-energy industries, but it has not been effectively developed and utilized because of degumming problems. To effectively take advantage of kenaf resources, to satisfy the growing demand for natural fiber, and to provide support for other fiber material degumming, steam explosion (STEX) pretreatment followed by alkali-oxygen treatment was studied. The effect of pressure on the properties of kenaf during the STEX treatment was studied, and the optimal degumming process for kenaf was selected. Results showed that STEX pretreatment removed pectin and part of the hemicellulose. Carbohydrates (cellulose and hemicellulose) could be degraded via high pressure treatment. The residual gum content and the fineness of the kenaf fiber after the alkali-oxygen treatment were good enough for textile production. High pressure was found not to be a key factor influencing the degumming process. Low pressure STEX (0.5 MPa) and alkali-oxygen treatment was judged to be an efficient method for degumming kenaf fibers.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.