Abstract

Aim of this in vitro study was to compare self-etch adhesives regarding microtensile bond strength (μ-TBS) to dentin of primary teeth. Fifty freshly extracted primary molars were ground to expose caries-free dentin. Specimens were bonded with ten self-etch adhesives (iBond self-etch/Heraeus, Xeno V+/Dentsply, G-Bond, Gaenial Bond/GC, BeautiBond/Shofu, AdheSE One F/Ivoclar Vivadent, Adper Easy Bond/3M ESPE, Clearfil SE Bond/Kuraray, OptiBond XTR/KerrHawe, Prime&Bond NT/Dentsply). After 24-h storage (distilled water, 37°C), resin-dentin beams were cut and 848 resin-dentin sticks were subjected to μ-TBS tests. Fracture analysis was carried out at 40× magnification under a fluorescence microscope and under a SEM. Three adhesives (iBond SE, Clearfil SE Bond, Prime&Bond NT) did not suffer pre-test failures (PTF). AdheSE One F revealed the largest portion of PTF (28%; P<0.05). Clearfil SE Bond and OptiBond XTR exhibited more cohesive fractures than the other adhesives (77.3% vs 64.8%; P<0.05). iBond SE, Gaenial Bond, Clearfil SE, and OptiBond XTR achieved μ-TBS of >60MPa, whereas Xeno V+ and AdheSE One F ranged only at ~20MPa (P<0.05). Within the limits of this study, the self-etch adhesives under investigation proved different extents of initial μ-TBS to primary dentin with iBond SE, Gaenial Bond, Clearfil SE, and OptiBond XTR having been most successful.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.