Oxide-supported single-atom Pt materials are prepared by combining surface organometallic chemisorption with atomic layer deposition (ALD). Here Pt is supported as a discrete monatomic “pincer” complex, stabilized by an atomic layer deposition (ALD) derived oxide overcoat, and then calcined at 400 °C under O2. ALD-derived Al2O3, TiO2, and ZnO overlayers are effective in suppressing Pt sintering and significantly stabilizing single Pt atoms. Furthermore, this procedure decreases the overall Pt nuclearity (∼1 nm average particle diameter) versus bare Pt (∼3.8 nm average diameter), as assayed by aberration corrected HAADF-STEM. The TiO2 and ZnO overcoats are significantly more effective at stabilizing single-atom Pt species and decreasing the overall Pt nuclearity than Al2O3 overcoats. Vibrational spectroscopy of adsorbed CO also shows that oxidized Pt species commonly thought to be single Pt atoms are inactive for catalytic oxidation of adsorbed CO. CO chemisorption measurements show site blockage by the AL...
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.