We report the synthesis of large-area, high-Ti-content, Mo1−xTixS2 alloy thin films in the 2H phase at temperature as low as 500 °C using a scalable two-step method of metal film deposition, followed by sulfurization in H2S. Film processing at higher temperature accelerates Ti segregation, film coarsening, and the formation of TiS2 in the 1T phase. Crystal growth at higher temperature results in the formation of multiple binary sulfide phases, in agreement with the equilibrium phase diagram. Making highly metastable, smooth, and uniform single-phase alloy films, therefore, hinges on developing low-temperature processing. Our results are relevant to the development of technologies based on designer transition metal dichalcogenide alloys, including in photonic integrated circuits and gas sensing.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.