Abstract Nanoparticles of stabilized ZrO2 in a single cubic phase by 5–20 at.% (of total metal cations) Cr3+/Cr4+ addition are obtained through a chemical method using a polymer matrix made of sucrose and polyvinyl alcohol. On heating at 250–900 °C in air, the polymer network decomposes and burns out leaving behind a dispersed microstructure in 10–25 nm diameter particles of cubic ZrO2 in spherical shape. A modified microstructure comprises of 10–14 nm crystallites of dispersed tetragonal phase, or both tetragonal and monoclinic phases, in cubic phase appear on a prolong (2 h or larger) heating of precursor at 900–950 °C. Particles in tetragonal ZrO2 are in acicular shape, while the monoclinic phase is in the shape of platelets. The Cr3+/Cr4+ additive facilitates formation of cubic phase in small particles on a controlled decomposition and combustion of precursor. It stabilizes small particles by inhibiting their growth by forming a thin amorphous surface layer over them.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.