Measurements of the linear permittivity and third-order harmonic generation were carried out for KNO 3 loaded molecular sieves MCM-41 with pores of 37 and 26 Å in comparison with bulk potassium nitrate. The samples were warmed up to 423 and 463 K from room temperature. The ferroelectric phase III was shown to occur upon cooling in both nanocomposites after warming till 463 K when it emerges also in bulk KNO 3. Nanoconfinement led to the pronounced broadening of the temperature range of ferroelectricity. While under the thermal conditions when phase III does not arise in bulk KNO 3, ferroelectricity was found only within pores of 26 Å.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.