Effective solidification/stabilization (S/S) of arsenic- and barium-containing D004/D005 waste was accomplished by using a binder of cement with 40% class C fly ash and either ferrous sulfate or ferric sulfate as an additive. Addition of iron salts improves arsenic solidification/stabilization (S/S). Barium may be encapsulated within the stabilized matrix as barium sulfate. Recommended mole ratios for iron/arsenic and barium/sulfate are at least 6 and 1.2, respectively. A binder/waste ratio of 0.15 is volume efficient, but the mix design must be carefully controlled to achieve adequate S/S. In practice, the heterogeneity of waste and large-scale mix operations may preclude close control of reagent dosages, so a binder/waste ratio of 0.40 is preferable. Ferrous sulfate additive is preferable for arsenic S/S because it is effective over a wider range of mix designs and over a long-term curing period. Toxicity characteristic leaching procedure results degraded with long curing time for some mix designs with ferric sulfate additive.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.