Abstract
In the paper, hydrothermal treatment (HT) of MSWI fly ashes was performed to stabilize and separate heavy metals. Influences of pre-treatment, types of ferric and/or ferrous additives, and subsequent heavy metal stabilization procedure by adding phosphate were investigated. The chemical stability of hydrothermal products was examined by solid waste extraction procedure with acetic acid buffer solution. Mineralogical investigation of selected hydrothermal product was carried out by XRD. FEGE SEM- -EDX was used to study the morphology and surface compositions of the ash particles. Experimental results revealed that HT process facilitated heavy metal exposure to leaching solution. FEGE SEM-EDX images revealed that fly ash particles were re-organized during hydrothermal process and that the minerals with special shapes and containing high levels of heavy metals were formed. A mild acid washing treatment with final pH around 6.20 could remove soluble heavy metals. Therefore, it may be a proper pre- or post-treatment method for fly ash particles for the purpose of reducing heavy metal contents. For the purpose of stabilizing heavy metals, the addition of ferric/ferrous salts in the HT process or phosphate stabilization after HT is recommended. The HT process may be applied to realize the environmentally sound management of MSWI fly ash or to recover and utilize MSWI fly ash.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.