Experimental laboratory tests were performed using volcanic glasses from Argentina of variable chemical composition and texture, in 1 N KOH, NaOH, Ca(OH)2 and combined NaOH + KOH + Ca(OH)2 solutions, at 40 °C and up to 10 weeks. The initial materials were characterized by petrography, chemical analysis, XRD, FT-IR and DSC-TGA. The reaction progress was evaluated by XRD, and the final products studied by SEM-EDS. The reactivity of the most reactive glass is attributed to a combination of its high porosity/permeability and alteration degree (indirectly assessed by the volatile mass loss up to ~250 °C). The glass silica content and Ca/(Al+Si) ratio could be other factors affecting the glass reactivity; however, more studies are needed to understand the influence of these variables.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.