In this article, we have reported hexagonal phase of SrAl2O4 (SAO) at room temperature by synthesizing ZnO-SAO nanocomposite which has been found to be difficult to achieve. Through combustion technique, we have made ZnO(20%)-SAO(80%) nanocomposite and revealed a good dispersion of ZnO in SAO matrix. A stable hexagonal phase at RT has been obtained in the composite sample calcined at 700 and 800 °C. Further, increasing the calcination temperature to 1000 and 1200°C, hexagonal phase transforms to monoclinic. From photoluminescence studies, we have observed an emission close to white light with changing the calcination temperature.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.