β-SiC-particle-dispersed-aluminum (Al) matrix composite was fabricated in the solid-liquid co-existent state by the Spark Plasma Sintering (SPS) process from the mixture of β-SiC powders, Al powders and Al-5 mass% Si powders. The microstructures and thermal conductivities of the composites fabricated were examined. These composites were all well consolidated by heating at a temperature range between 798 K and 876 K for 1.56 ks during the SPS process. No reaction at the interface between the β-SiC particle and the Al matrix was observed by scanning electron microscopy for the composites fabricated under the sintering conditions employed in the present study. The relative packing density of the Al/β-SiC composite fabricated was higher than 99 % in a volume fraction range of SiC between 40 % and 50 %. Thermal conductivity of the Al/β-SiC composite was higher than 200 W/mK in a β-SiC volume fraction range between 40 and 50 vol%. The highest thermal conductivity was obtained for Al-45 vol% β-SiC composite and reached 216 W/mK. The coefficient of thermal expansion of the composites falls in the upper line of Kerner's model, indicating strong bonding between the β-SiC particle and the Al matrix in the composite.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call