Spark plasma sintering (SPS) method was used to sinter two different types of 93W-5.6Ni-1.4Fe (wt pct) heavy alloy powders which were respectively prepared by simple mixing and high-energy ball milling (HEBM) for 40 h. In SPS processing, the powder compacts were heated at 100 °C/min to the desired sintering temperature with 5 min holding. The SPS densification behavior of the two types of powders was investigated. For the simple mixed powders, the compacts start to shrink around 850 °C, and the densification is enhanced by diffusion and plastic deformation with the increase of temperature. Consequently the compacts shrink effectively and obtain nearly full density around 1230 °C. While for the as-milled powders, recovery and recrystallization occur between 700–850 °C due to the crystal lattice distortion and defects resulted from HEBM, causing the soften of particles and a slight shrink of compacts. When increasing temperature, nanosintering of W crystallines in the matrix occurs in the inside of the composite powders, and the densification rate accelerates and maximizes at about 1050 °C. Owing to the improved activity of powders from HEBM, the tungsten grains coarsen rapidly in the sintering, simultaneously, the harmful intermetallic phases Ni2W4C and Fe6W6C are generated.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call