Abstract

In this study, the springback characteristics of tailor-welded strips in U-bending processing were investigated. The tailor-welded strips were joined by the laser welding process and consisted of two types of thickness combinations of the SCP1 sheet, 0.8 t×1.2 t and 0.8 t×1.6 t, to investigate the effect of different thickness combination on the springback. And two different welded strips, one was welded along the centerline of the strip-width and the other was welded along the centerline of strip-length, were adopted to compare the effects of weld-line locations on the springback. Three punch profile radii of 3, 9 and 15 mm were used. Some selected cases from the experiments were simulated using a commercial finite element program, PAM-STAMP. In cases of the longitudinally welded strips, the springback was generated as much as the one generated in the non-welded strips, which are the same thickness as the thicker side of the longitudinally welded strips. And, in the cases of the centrally welded strips, a significant reduction of the springback was observed in the thinner side compared with the same thickness of non-welded strip. On the other hand, the springback of the thicker side was similar to the one of the same thickness non-welded strips.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.