Abstract

Spherical SrMoO4:Eu3+ phosphors had been prepared by spray pyrolysis. The effect of the total solution concentration on phase structure, microscopic morphology and fluorescent performances of SrMoO4: Eu3+ phosphor have been studied. The results showed that pure SrMoO4 phase can be obtained at different total solution concentration; The luminous intensity of the sample was the strongest at 615nm when the total solution concentration is 0.6M. SrMoO4: Eu3+ phosphor with regular spherical morphology, well dispersion and well fluorescent properties was synthesized successfully by spray pyrolysis method.