Abstract
The temperature dependence of the principal values of the refractive index in Sr1−xCaxTiO3 (x=0.014) has been measured in the 17–275 K range under various conditions of sample illumination with 1.96 eV photons. The spontaneous photorefractive contribution δnph to the temperature-induced variation of the refractive index of Sr1−xCaxTiO3, which appears after illumination of the sample in the ferrophase (transition temperature Tc=32 K) and persists in the paraphase under heating up to 150 K, has been separated. The photoinduced polarization has been estimated.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.