Abstract
This paper reports that Ta50W50 alloy has a higher spin Hall angle than that of β-W by measuring the spin Seebeck coefficients for Fe5Y3O12 (YIG)/Ru/Ta50W50 and YIG/Ru/W systems. The spin Seebeck coefficient increased by inserting Ru, and the YIG/Ru/Ta50W50 system achieved 2.4 times the magnitude of spin Seebeck coefficient of the conventional YIG/Pt system although Ru and Ta50W50 have spin Hall angles with opposite signs. Ru seems to recover the spin mixing conductance that is decreased by Ta–W oxidation at its interface with YIG. To enhance the spin Seebeck coefficient, materials having a high spin Hall angle can be combined with materials having a high spin mixing conductance.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.