Various zinc oxide films were deposited by ion-beam sputter deposition (IBSD) under different oxygen partial pressures (P(O2)) at room temperature. The as-deposited ZnO films fabricated at P(O2)>1.0×10(-4) Torr had poly-crystalline structures to absorb water on the surface at ambient condition. Simultaneously, the film surfaces were covered and smoothed by the surface layers formed with the water, hydroxyl (OH(-)) groups, and ZnO materials investigated by X-ray photoelectron spectroscopy (XPS). When the compositions of the surface layers were used in a multilayer fitting model of spectroscopic ellipsometry, the actual optical refractive index of the ZnO film deposited at P(O2)=1.2×10(-4) Torr was found to be about 1.9618 at λ=550 nm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.