Abstract

Research results on the specific heat of TlIn1−xCexS2 (0⩽x⩽0.04) crystals in the temperature range 4.2–300 K are presented. It is found that TlIn1−xCexS2 crystals have a second-order phase transition in the temperature interval 173.4–214 K, and the sharpness of the specific-heat peaks decreases gradually as cerium is substituted for indium in TlInS2.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.