Abstract

Specific contact resistances between an amorphous oxide semiconductor, In–Ga–Zn–O, and various metallic electrodes, Ag, Au, In, Pt, Ti, polycrystalline indium tin oxide (ITO) and amorphous indium zinc oxide (a-IZO), were examined. All the contacts except for Au and Pt showed linear current–voltage characteristics, while Au and Pt did Schottky contacts. Low contact resistances < 10 − 4 Ω cm 2 were obtained for the Ag, In, Ti, ITO and a-IZO contacts, and there is a trend that the contact resistance decreases with decreasing the work function of the metallic electrode. The performances of thin film transistors using ITO and Ti for source and drain contacts were better than that using the Schottky Au contacts. It was also found that the Ti contacts have a large distribution in the contact resistance, suggesting that a higher reproducibility process should be employed when reactive metals are used for an electrical contact to an oxide semiconductor.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call