Abstract

The metallurgical special features of the electroslag process using low-activity fluxes with the reduced basicity are investigated. The increase in the silica content of the fluxes–slags up to 15–25% improves the technological characteristics of the electroslag process and ensures efficient desulphurization of metal. When the silica content of the slag is increased above 25%, the oxygen content and the content of the non-metallic inclusions in the remelted metal rapidly increase.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.