Abstract

In this paper spark plasma sintering (SPS) of silicon carbide and multi-walled carbon nanotube reinforced zirconium diboride ultra-high temperature ceramic matrix composites is reported. Systematic investigations on the effect of reinforcement type (SiC and CNTs) and content (10–40vol.% SiC and 2–6vol.% CNTs) on densification behavior, microstructure development, and mechanical properties (microhardness, bi-axial flexural strength, and indentation fracture toughness) are presented. With the similar SPS processing parameters (1900°C, 70MPa pressure, and 15min soaking time), near-full densification (>99% relative density) was achieved with 10–40% SiC (in ZrB2–SiC) and 4–6% CNT (in ZrB2–CNT) reinforced composites. The SiC and CNT reinforcement further improved the indentation fracture toughness of the composites through a range of toughening mechanisms, including particle shearing, crack deflection at the particle-matrix interface, and grain pull-outs for ZrB2–SiC composites, and CNT pull-outs and crack deflection in ZrB2–CNT composites.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.