Investigated was the spark plasma sintering (SPS) of β-SiAlON/0–30 wt % BN ceramic composites. The raw materials (β-Si5AlON7 and BN powders) were prepared by infiltration-mediated combustion synthesis (CS). Experimentally established were the following process parameters for SPS of composites with high relative density (>95%) and flexural strength of 250–300 MPa: (a) heating rate 50 deg/min, (b) maximum temperature 1650–1750°C, (c) and holding time 5 min.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.