Abstract
Spark plasma sintering technique was used for the consolidation of nanostructured titanium carbide synthesized by mechanical alloying in order to avoid any important grain growth of the compact materials. The TiC phase was obtained after about 2 h of mechanical alloying. Towards the end of the milling process (20 h), the nanocrystalline powders reached a critical size value of less than 5 nm. Some physical and mechanical properties of the consolidated carbide were reported as a function of the starting grain size powders obtained after different mechanical alloying durations. The crystalline grain size of the bulk samples was found to be increased to a maximum of 120 nm and 91 nm for carbides mechanically alloyed for 2 h and 20 h respectively. The Vickers hardness showed to be improved to about 2700 Hv for a maximum density of 95.1% of the bulk material.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: International Journal of Refractory Metals and Hard Materials
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.