Abstract
TaC–4wt.% CNT composites were synthesized using spark plasma sintering. Two kinds of CNTs, having long (10–20μm) and short (1–3μm) length, were dispersed by wet chemistry and spray drying techniques respectively. Spark plasma sintering was carried out at 1850°C at pressures of 100, 255 and 363MPa. Addition of CNTs leads to an increase in the density of 100MPa sample from 89% to 95%. Short CNTs are more effective in increasing the density of the composites whereas long CNTs are more effective grain growth inhibitors. The longer CNTs are more effective in increasing the fracture toughness and an increase up to 60% was observed for 363MPa sample. Hardness and elastic modulus are found to increase by 22% and 18% respectively for 100MPa samples by addition of long CNTs. Raman spectroscopy, SEM and TEM images indicated that the CNTs were getting transformed into flaky graphitic structures at pressure higher than 100MPa.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.