Abstract

We report a new ‘spark erosion’ technique for producing high-quality thermoelectric nanoparticles at a remarkably high rate and with enhanced thermoelectric properties. The technique was utilized to synthesize p-type Bi0.5Sb1.5Te3 nanoparticles with a production rate as high as 135 g h−1, using a relatively small laboratory apparatus and low energy consumption. The compacted nanocomposite samples made from these nanoparticles exhibit a well-defined, 20–50 nm size nanograin microstructure, and show an enhanced figure of merit, ZT, of 1.36 at 360 K. Such a technique is essential for providing inexpensive, oxidation-free nanoparticles which are required for the fabrication of high performance thermoelectric devices for power generation from waste heat, and for refrigeration.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.