Abstract

When apatites and phosphorites are processed, up to 30% of rare earth metals are converted into wet-process phosphoric acid. Wet-process phosphoric acid from the phosphorite treatment process differs from apatite one by impurity composition, i.e. the iron content is by 3.5 times, and calcium is by 5.0 times more. The complex composition of the wet-process phosphoric acid from the phosphorite treatment process requires additional researches to select optimal ion exchangers and technological parameters of sorption. Various aspects of sorption have been studied to select the optimal ion exchangers and technological parameters, and technological modes for desorption of rare earth metals from a cation exchanger to obtain a concentrate of rare earth metals have been completed. The method enables to extract rare earth metals without changing the composition of commercial wet-process phosphoric acid directly in the production process of the enterprises engaged in the phosphorite treatment process.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.