Abstract

Pure Aluminium mixed with SiC powder (size 70 micron) in 5, 10 , 15 and 20 percentage weight fractions have been stir cast and test samples have been made. The samples have been machined to produce 8 mm diameter pins for testing in Pin on Disc wear monitor under water lubricated condition. The wear behaviour of these samples has been studied by plotting the wear rates against sliding distance and velocity. The co efficient of friction has been found out under varying load and varying time. The results were compared with that of pure aluminium under similar test conditions. It has been found that the sample having 20% weight fraction of SiC with highest hardness has maximum wear resistance under such conditions.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.