Abstract

Abstract Well-dispersed cerium-doped Y2SiO5 (Ce:YSO) phosphor particles with spherical morphology and good luminescence intensity have been achieved by a solvothermal method with ethanol and water as solvent media. X-ray diffraction, Fourier transform infrared spectroscopy, fluorescence spectrophotometry and transmission electron microscopy were employed to characterize the as-synthesized Ce:YSO precursor and powders. The results showed that pure-phase Ce:YSO powders with a mean particle size of about 162 nm were accurately available at 310°C and above. The fluorescence ability and persistent luminescence decay properties of the Ce:YSO powders were also studied, and the excellent fluorescence properties could be attributed to the homogeneous Ce:YSO particles obtained through the solvothermal method.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.