Abstract

Preparation of FePt nanowires by thermal decomposition of the solution mixture of equimolar Fe(CO)5 and Pt(acac)2 in n-octylamine will be presented in this account. The nanowires with the average diameter about 2 nm and the length of several hundred nanometers were characterized by TEM, EDS, XRD. It is believed that FePt nanowires were generated via the catalytic solution-liquid-solid (S-L-S) synthetic approach. This process is strongly dependent on the solvent and barely on the reaction temperature and the concentrations of precursors.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.