Abstract
Electrospinning is a well-known method to obtain nanofibers and collagen is a very attractive material for biological applications due to its bioactive nature. However, the preservation of the natural structure of collagen at the end products due to the different production parameters is an open question. In this study the importance of the preparation temperature for CD measurements and the solvent effect that employed in the electrospinning process was discussed. The decrease of the preparation temperature by 10° increased the measured PP-II (folded) fraction ratio from 37% to 52.5% and the nanofibers that were obtained from acidic solvent scored 59% of PP-II fraction ratio.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.