Abstract

To determine whether DMSO could serve as an effective pretreatment to improve the mechanical properties and minimize the degradation of the adhesive interface, through the degree of conversion (DC) and bond strength to dentin of different categories of dentin bonding systems (DBSs) after 30 months. DMSO (0, 0.5, 1, 2, 5, 10vol%) were incorporated into four categories of DBSs: Adper Scotchbond Multipurpose (MP), Adper Single Bond 2 (SB), Clearfil SE Bond (CSE) and Adper Scotchbond Universal (SU). DC was evaluated by Fourier transform infrared spectroscopy (FTIR). For microtensile bond strength test (µTBS), 1 % DMSO were applied on dentin as pretreatment before DBSs. For SU, both strategies were tested. Specimens for µTBS were tested after 24h, 6 and 30 months. DC and µTBS data were subjected to two-way ANOVA and Tukey test (α<0.05). Incorporating 5 %/10 % DMSO increased the DC of CSE. Controversially, when combined with SU, 2 % and 10 % DMSO jeopardized the DC. Regarding µTBS, 1 % DMSO pre-treatment increased the bond strength for MP, SB, SU-ER and SU-SE. After 30 months, MP, SU-ER and SU-SE showed a decrease compared to baseline but remained higher than the control. DMSO pretreatment may be a useful strategy to improve the bond interface over time. Its incorporation seems to favor the non-solvated systems regarding DC while it seems to show long-term benefits for bond strength using 1 % DMSO for MP and SU systems.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.