Abstract
A ZnO transistor with carrier mobility of 3 cm2 V−1 s−1 using a SiO2 insulator formed at low-temperature (180 °C) from solution-processed perhydropolysilazane.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.