Abstract

A viscous Nickel (Ni) solution was applied on amorphous Si films by spin coating and its effect on the crystallization of amorphous Si films was investigated with a two-step annealing process. The experimental results show that with the help of the two-step annealing, the crystallization of the film can take place at 500oC. At the same time, the crystalline fraction gets up to 79.4% after annealing at a high temperature of 520oC and the grain size of the polycrystalline Si films is approximately 200 nm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.