The solubility limits of important dopants (La and Y) in aluminum oxynitride (AlON) were measured using wavelength‐dispersive spectroscopy (WDS) mounted on a scanning electron microscope, from samples quickly cooled from 1870°C. To provide saturated AlON, samples were prepared with dopant concentrations well above the solubility limit, which was confirmed by the appearance of secondary phases using X‐ray diffraction, backscattered electron micrographs, and WDS. Measurements were conducted on polished samples without thermal or chemical etching. The results indicate solubility limits of 498±82 and 1775±128 ppm for La and Y in AlON at 1870°C, respectively. The solubility limit of Mg in AlON at 1870°C was found to be >4000 ppm. The relation between solubility limit and cation size is briefly discussed.
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.