Abstract
AbstractSolid‐state lithium–sulfur battery (SSLSB) is attractive due to its potential for providing high energy density. However, the cell chemistry of SSLSB still faces challenges such as sluggish electrochemical kinetics and prominent “chemomechanical” failure. Herein, a high‐performance SSLSB is demonstrated by using the thio‐LiSICON/polymer composite electrolyte in combination with sulfurized polyacrylonitrile (S/PAN) cathode. Thio‐LiSICON/polymer composite electrolyte, which processes high ionic conductivity and wettability, is fabricated to enhance the interfacial contact and the performance of lithium metal anodes. S/PAN is utilized due to its unique electrochemical characteristics: electrochemical and structural studies combined with nuclear magnetic resonance spectroscopy and electron paramagnetic resonance characterizations reveal the charge/discharge mechanism of S/PAN, which is the radical‐mediated redox reaction within the sulfur grafted conjugated polymer framework. This characteristic of S/PAN can support alleviating the volume change in the cathode and maintaining fast redox kinetics. The assembled SSLSB full cell exhibits excellent rate performance with 1183 mAh g−1 at 0.2 C and 719 mAh g−1 at 0.5 C, respectively, and can accomplish 50 cycles at 0.1 C with the capacity retention of 588 mAh g−1. The superior performance of the SSLSB cell rationalizes the construction concept and leads to considerations for the innovative design of SSLSB.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.